Uniaxial and Triaxial Creep Test

Creep Test

 

Equipment required for this test is as follows:

  • Loading device for applying and controlling axial load
  • Triaxial cell:
  • A triaxial cell to apply confining pressure to the specimen
  • Platens both specimen ends
  • Spherical seats shall be located in each of the platens
  • A flexible membrane of suitable material shall be used to prevent the confining fluid from entering the specimen
  • Device for applying confining pressure
  • Equipment for measuring and recording loads, pressures and displacements

 

Capabilities of Creep test apparatus:

  • Maximum load force: 500 ton
  • Maximum confining pressure 80 MPa
  • Equipped with data Acquisition system

 

Creep Test

Creep Test

Triaxial Compression testHydraulic Fracturing Test